Table 1
Arachidy-l-behenyl amide (C20-C22fatty acid amides) |
5 percent. |
Azodicarbonamide |
1. 2 percent. |
|
2. 5 percent; for use only in the manufacture of polyethylene complying with item 2.1 in § 177.1520(c) of this chapter. |
Balata rubber |
Benzyl alcohol |
1 percent. |
Brominated isobutylene-isoprene copolymers, produced when isobutylene-isoprene copolymers complying with § 177.1420(a)(2)
are modified by bromination with not more than 2.3 weight-percent of bromine and having a Mooney Viscosity (ML 1 8 (125 °C)) of 27 or higher. The viscosity is determined by the American Society for Testing and Materials (ASTM) method D 1646-81, “Standard Test Method for Rubber—Viscosity and Vulcanization Characteristics (Mooney Viscometer),” which is incorporated by reference in accordance with
5 U.S.C. 522(a)
and 1 CFR part 51
. Copies are available from the AOAC INTERNATIONAL, 481 North Frederick Ave., Suite 500, Gaithersburg, MD 20877-2504 and the Center for Food Safety and Applied Nutrition (HFS-200), Food and Drug Administration, 5100 Paint Branch Pkwy., College Park, MD 20740, or available for inspection at the National Archives and Records Administration (NARA). For information on the availability of this material at NARA, call 202-741-6030, or go to: http://www.archives.gov/federal_register/code_of_federal_regulations/ibr_locations.html.
|
1,3-Butanediol |
Calcium tin stearate |
2 percent. |
Calcium zinc stearate |
Do. |
Carbon, activated |
1 percent. |
Castor oil, hydrogenated |
2 percent. |
Chlorinated isobutylene-isoprene copolymers complying with § 177.1420
|
Coco amide (coconut oil fatty acids amides) |
2 percent. |
Cork (cleaned, granulated) |
Diebenzamide phenyl disulfide |
1 percent; for use only in vulcanized natural or synthetic rubber gasket compositions. |
Di(C7, C9-alkyl) adipate |
Complying with § 178.3740 of this chapter; except that, there is no limitation on polymer thickness. |
Di-2-ethylhexyl adipate |
Di-2-ethylhexyl sebacate |
2 percent. |
Di-2-ethylhexyl terephthalate (CAS Reg. No. 006422-86-2). |
For use as a plasticizer at levels not exceeding 75 parts per hundred by weight of permitted vinyl chloride homo- and/or copolymer resins used in contact with food of Types I, II, IV-B, VI-A, VI-B, VI-C (up to 15 percent alcohol by volume), VII-B, and VIII described in § 176.170(c) of this chapter, table 1, and under conditions of use A through H described in § 176. 170 (c) of this chapter, table 2. |
Dihexyl ester of sodium sulfosuccinate |
1 percent. |
Diisodecyl phthalate |
No limitation on amount used but for use only in closure-sealing gasket compositions used in contact with non-fatty foods containing no more than 8 percent of alcohol. |
Di-β-naphthyl-p-phenylenediamine |
1 percent. |
Dipentamethylenethiurametetrasulfide |
0.4 percent; for use only in vulcanized natural or synthetic rubber gasket compositions. |
Eicosane (technical grade) (water-white mixture of predominantly straight-chain paraffin hydrocarbons averaging 20 carbon atoms per molecule) |
Epoxidized linseed oil |
Epoxidized linseed oil modified with trimellitic anhydride |
Epoxidized safflower oil |
Epoxidized safflower oil modified with trimellitic anhydride |
Epoxidized soybean oil modified with trimellitic anhydride |
Erucylamide |
5 percent. |
Code of Federal Regulations
255
|
Ethylene-propylene copolymer |
Ethylene-propylene modified copolymer elastomers produced when ethylene and propylene are copolymerized with 5-methylene-2-norbornene and/or 5-ethylidine-2-norbornene. The finished copolymer elastomers so produced shall contain not more than 5 weight-percent of total polymer units derived from 5-methylene-2-norbornene and/or 5-ethylidine-2-norbornene, and shall have a minimum viscosity average molecular weight of 120,000 as determined by the method described in § 177.1520(d)(5)
, and a minimum Mooney viscosity of 35 as determined by the method described in § 177.1520(d)(6)
|
Ethylene-vinyl acetate copolymer |
Glyceryl mono-12-hydroxystearate (hydrogenated glyceryl ricinoleate) |
2 percent. |
Gutta-percha |
Hexamethylenetetramine |
1 percent. |
Hexylene glycol |
0.5 percent. |
Isobutylene-isoprene copolymers complying with § 177.1420
|
Maleic anhydride-polyethylene copolymer |
5 percent. |
Maleic anhydride-styrene copolymer |
Do. |
2,2′-Methylenebis[6-(1-methylcylcohexyl)-p-cresol] |
1 percent. |
Mixed octylated diphenylamine (CAS Reg. No. 68411-46-1) |
0.1 percent in isobutylene-isoprene and chlorinated isobutylene-isoprene copolymers complying with § 177.1420
, and brominated isobutylene-isoprene copolymers complying with this section. |
Napthalene sulfonic acid-formaldehyde condensate, sodium salt |
0.2 percent. |
Natural rubber (crepe, latex, mechanical dispersions) |
α-cis-9-Octadecenyl-omega-hydroxypoly (oxyethylene); the octadecenyl group is derived from oleyl alcohol and the poly (oxyethylene) content averages 20 moles |
0.5 percent. |
Oleyl alcohol |
1 percent. |
4,4′-Oxybis (benzene sulfonyl hydrazide) |
0.5 percent. |
Paraformaldehyde |
1 percent. |
Polybutadiene |
Poly-p-dinitroso benzene (activator for butyl rubber) |
1 percent; for use only in vulcanized natural or synthetic rubber gasket compositions. |
Polyethylene glycol 400 esters of fatty acids derived from animal and vegetable fats and oils |
1 percent. |
Polyisobutylene complying with § 177.1420
|
Polyoxypropylene-polyoxyethylene condensate, average mol. wt. 2750-3000 |
0.05 percent. |
Polyurethane resins manufactured from diphenylmethane diisocyanate, 1,4-butanediol, and adipic acid (CAS Reg. No. 26375-23-5). |
For use only:No limitation on amount used, but for use only in closure gasket compositions used in contact with food types VI-A and VI-C (up to 15 percent alcohol) under conditions of use D, E, F, and G, as described in § 176.170(c) of this chapter, tables 1 and 2, respectively.
|
Potassium benzoate |
1 percent. |
Potassium perchlorate |
Do. |
Potassium propionate |
2 percent. |
Potassium and sodium persulfate |
1 percent. |
Resorcinol |
0.24 percent; for use only as a reactive adjuvant substance employed in the production of gelatin-bonded cord compositions for use in lining crown closures. The gelatin so used shall be technical grade or better. |
Rosins and rosin derivatives as defined in § 175.300(b)(3)(v) of this chapter for use only in resinous and polymeric coatings on metal substrates; for all other uses as defined in § 178.3870 of this chapter
|
Sodium cetyl sulfate |
1 percent. |
Sodium decylbenzenesulfonate |
Do. |
Sodium decyl sulfate |
Do. |
Sodium formaldehyde sulfoxylate |
0.05 percent. |
Sodium lauryl sulfate |
1 percent. |
Sodium lignin sulfonate |
0.2 percent. |
Sodium myristyl sulfate (sodium tetradecyl sulfate) |
0.6 percent. |
Sodium nitrite |
0.2 percent; for use only in annular ring gaskets applied in aqueous dispersions to closures for containers having a capacity of not less than 5 gallons. |
Code of Federal Regulations
256
|
Sodium o-phenylphenate |
0.05 percent. |
Sodium polyacrylate |
5 percent. |
Sodium and potassium pentachlorophenate |
0.05 percent. |
Sodium salt of trisopropyl napthalenesulfonic acid |
0.2 percent. |
Sodium tridecylsulfate |
0.6 percent. |
Stearic acid amide |
5 percent. |
Sulfur |
For use only as a vulcanizing agent in vulcanized natural or synthetic rubber gasket compositions at a level not to exceed 4 percent by weight of the elastomer content of the rubber gasket composition. |
Tallow, sulfated |
1 percent. |
Tin-zinc stearate |
2 percent. |
Tri(mixed mono- and dinonylphenyl) phosphite |
1 percent. |
Vinyl chloride-vinyl stearate copolymer |
Zinc dibutyldithiocarbamate |
0.8 percent; for use only in vulcanized natural or synthetic rubber gasket compositions. |